粉末特征对激光粉末床熔融制备可降解Zn-Mn-Mg合金组织与力学性能的影响 |
| 黄成聪, 李亚庚, 王鲁宁 |
|
Effects of Powder Morphology on Microstructure Evolution and Mechanical Properties of Laser Powder Bed Fusion Degradable Zn-Mn-Mg Alloy |
| HUANG Chengcong, LI Yageng, WANG Luning |
| 图2 EIGA方法制备的合金粉末经不同激光粉末床熔融(LPBF)工艺成形后的块体试样的致密度等高线图和OM像 |
| Fig.2 Contour diagram of relative density (a) and OM images of laser powder bed fusion (LPBF) bulk samples prepared via EIGAed powders at P = 40 W, V = 900 mm/s (b), P = 70 W, V = 900 mm/s (c), P = 40 W, V = 800 mm/s (d), P = 80 W, V = 900 mm/s (e), P = 50 W, V = 600 mm/s (f), P = 80 W, V = 600 mm/s (g), P = 40 W, V = 500 mm/s (h), P = 50 W, V = 500 mm/s (i), P = 60 W, V = 600 mm/s (j), P = 70 W, V = 700 mm/s (k), and P = 80 W, V = 800 mm/s (l) (P—laser power, V—scanning rate) |
|