粉末特征对激光粉末床熔融制备可降解Zn-Mn-Mg合金组织与力学性能的影响
黄成聪, 李亚庚, 王鲁宁

Effects of Powder Morphology on Microstructure Evolution and Mechanical Properties of Laser Powder Bed Fusion Degradable Zn-Mn-Mg Alloy
HUANG Chengcong, LI Yageng, WANG Luning
图1 EIGA和PREP方法制备的Zn-Mn-Mg合金粉末的SEM像和尺寸分布
Fig.1 SEM images (a, b) and particle size distributions (c, d) of Zn-Mn-Mg alloy powders prepared by EIGA (a, c) and PREP (b, d) methods (Dv(10), Dv(50), and Dv(90) indicate 10%, 50%, and 90% cumulative particle sizes, respectively)