细观力学模拟双峰晶粒分布铜的异质变形诱导效应
|
|
李少杰, 金剑锋, 田艳中, 潘虎成, 王明涛, 秦高梧
|
Micromechanics Modeling of the Hetero-Deformation Induced Strengthening and Strain Hardening Effect in Bimodal Structure Copper
|
|
LI Shaojie, JIN Jianfeng, TIAN Yanzhong, PAN Hucheng, WANG Mingtao, QIN Gaowu
|
|
表1 双峰结构铜的材料和模拟参数
|
Table 1 Material parameters for bimodal structure Cu
|
|
| Parameter type | Symbol | Unit | Parameter value | Note |
|---|
| | | Hard zone | Soft zone | | | Elastic modulus | E | GPa | 121.1 | 121.1 | 1* | | Shear modulus | μ | GPa | 45.2 | 45.2 | | | Poisson's ratio | v | - | 0.34 | 0.34 | | | Burgers vector magnitude | b | nm | 0.256 | 0.256 | | | Taylor factor | M | - | 3.06 | 3.06 | | | Taylor constant | | - | 0.33 | 0.33 | | | Rate sensitivity exponent | m | - | 20 | 20 | | | Initial dislocation density | | m-2 | 6.7 × 1014 | 1.89 × 1013 | 2* | | Geometric factor | | - | 2.20 | 0.08 | | | Proportionality factor | | - | 0.150 | 0.013 | | | Dynamic recovery factor | | - | 39.8 | 1.31 | | | Size of zone | | μm | - | 6 | | | Dislocation pileup spacing | | nm | 15 | 42 | 3* | | Dynamic recovery factor of GNDs | | - | | 7 | | | Stress attenuation factor | λ | - | 0.1 | | | | Saturation accumulated shear strain | | - | 0.20 | - | |
|
|
|