李少杰, 金剑锋, 田艳中, 潘虎成, 王明涛, 秦高梧

Micromechanics Modeling of the Hetero-Deformation Induced Strengthening and Strain Hardening Effect in Bimodal Structure Copper
LI Shaojie, JIN Jianfeng, TIAN Yanzhong, PAN Hucheng, WANG Mingtao, QIN Gaowu
图2 软域硬化示意图
Fig.2 Schematics of soft zone hardening (σ—stress; ρ—density; ρ1G—GND density within soft zone; σ1G—isotropic hardening caused by GNDs within soft zone; σ1B—back stress caused by GNDs within soft zone; σ1M—incremental stress within soft zone; ρ0S, ρ1S—statistically stored dislocation density within hard zone and soft zone, respectively; σ0S, σ1S—isotropic hardening caused by statistically stored dislocations within hard zone and soft zone, respectively)
(a) schematic of the microstructure near the hetero-zone boundary
(b1, b2) TEM image of dislocation pile-ups within the soft zone (b1)[22] and schematic of GND distribution (b2) (The yellow lines are pile-ups of GNDs in a recrystallized grain after tensile deformation for a strain of 5%)
(c, d) dislocation density variation (c) and stress variation (d) near the black horizontal line at the hetero-zone boundaries in Fig.2a due to mismatch strengthening