Yb-Gd改性硅黏结层的高通量制备与耐腐蚀性能
|
|
王晔晗, 吕熙睿, 石金瑜, 雷一明, 张洁, 王京阳
|
High-Throughput Preparation and Corrosion Resistance of Yb-Gd Modified Si Bond Coat
|
|
WANG Yehan, LV Xirui, SHI Jinyu, LEI Yiming, ZHANG Jie, WANG Jingyang
|
|
表1 组合材料芯片在1300 ℃空气和水蒸气氧化1 h后特征点截面不同位置EDS半定量成分分析
|
Table 1 Semi-quantitative EDS composition analyses of different positions of the characteristic points on the cross-section of material chips after air and steam corrosion at 1300 oC
|
|
| Point | State | Position | Atomic fraction of element / % | RE / Si | Gd / Yb |
|---|
| Si | Gd | Yb | O |
|---|
| L4 | As-prepared | | 52.0 ± 0.8 | 32.6 ± 2.3 | 15.5 ± 1.5 | | 0.92 | 2.10 | | Air oxidation | Top layer | 14.3 ± 0.6 | 17.8 ± 0.7 | 8.6 ± 0.8 | 59.4 ± 0.8 | 1.85 | 2.07 | | Middle layer | 11.5 ± 0.4 | 17.4 ± 0.5 | 7.0 ± 0.3 | 64.1 ± 0.9 | 2.11 | 2.49 | | Bottom layer | 10.6 ± 0.7 | 16.9 ± 0.7 | 7.0 ± 0.2 | 65.5 ± 1.1 | 2.25 | 2.44 | | Steam corrosion | Top layer | 11.9 ± 1.5 | 16.7 ± 1.4 | 6.4 ± 0.5 | 65.1 ± 2.6 | 1.95 | 2.62 | | Middle layer | 10.2 ± 1.1 | 16.7 ± 1.4 | 6.3 ± 0.7 | 66.7 ± 3.0 | 2.25 | 2.64 | | Bottom layer | 7.2 ± 1.9 | 14.1 ± 3.1 | 5.8 ± 1.0 | 72.9 ± 0.3 | 2.78 | 2.44 | | F6 | As-prepared | | 62.5 ± 0.6 | 22.2 ± 0.3 | 15.3 ± 0.3 | | 0.60 | 1.45 | | Air oxidation | Top layer | 14.5 ± 1.1 | 16.7 ± 0.5 | 9.1 ± 0.6 | 59.7 ± 2.2 | 1.78 | 1.85 | | Middle layer | 12.3 ± 0.6 | 16.5 ± 0.6 | 8.8 ± 0.4 | 62.5 ± 1.4 | 2.04 | 1.88 | | Bottom layer | 9.8 ± 1.4 | 14.6 ± 0.9 | 7.9 ± 0.4 | 67.7 ± 2.5 | 2.29 | 1.85 | | Steam corrosion | Top layer | 10.7 ± 0.3 | 12.2 ± 0.3 | 6.5 ± 0.2 | 70.5 ± 0.4 | 1.76 | 1.87 | | Middle layer | 10.1 ± 0.9 | 13.3 ± 0.9 | 6.8 ± 0.4 | 69.8 ± 2.1 | 1.98 | 1.97 | | Bottom layer | 7.6 ± 1.2 | 13.2 ± 1.4 | 6.4 ± 0.5 | 72.8 ± 2.7 | 2.56 | 2.06 | | A2 | As-prepared | | 73.3 ± 5.0 | 13.9 ± 5.2 | 12.7 ± 0.3 | | 0.36 | 1.10 | | Air oxidation | Top layer | 17.3 ± 0.9 | 13.1 ± 0.9 | 8.3 ± 0.4 | 61.4 ± 1.3 | 1.23 | 1.58 | | Middle layer | 12.3 ± 0.9 | 13.3 ± 0.7 | 8.5 ± 0.1 | 65.9 ± 0.5 | 1.78 | 1.57 | | Bottom layer | 10.5 ± 1.1 | 10.6 ± 1.7 | 7.3 ± 1.0 | 71.5 ± 0.4 | 1.70 | 1.45 | | Steam corrosion | Top layer | 16.8 ± 2.0 | 12.0 ± 1.2 | 7.8 ± 0.4 | 63.5 ± 1.3 | 1.18 | 1.54 | | Middle layer | 11.0 ± 1.3 | 13.0 ± 1.1 | 7.8 ± 0.2 | 68.2 ± 0.9 | 1.91 | 1.67 | | Bottom layer | 10.4 ± 0.5 | 10.2 ± 0.7 | 6.7 ± 0.5 | 72.7 ± 1.4 | 1.62 | 1.52 |
|
|
|