Yb-Gd改性硅黏结层的高通量制备与耐腐蚀性能 |
| 王晔晗, 吕熙睿, 石金瑜, 雷一明, 张洁, 王京阳 |
|
High-Throughput Preparation and Corrosion Resistance of Yb-Gd Modified Si Bond Coat |
| WANG Yehan, LV Xirui, SHI Jinyu, LEI Yiming, ZHANG Jie, WANG Jingyang |
| 图7 1300 ℃水氧腐蚀后,芯片氧化膜生长率随成分的变化、微区XRD谱以及表面和截面的SEM像 |
| Fig.7 Variation of oxide film growth rate with composition changes (a); micro-XRD patterns of material chips after water vapor corrosion at 1300 oC (b); and surface (c, e, g) and cross-sectional (d, f, h) SEM images of L4 (c, d), F6 (e, f), and A2 (g, h) sample patches on the material chips after steam corrosion at 1300 oC (Insets in Figs.7c, e, and g are the corresponding enlarged images) |
|