Yb-Gd改性硅黏结层的高通量制备与耐腐蚀性能 |
| 王晔晗, 吕熙睿, 石金瑜, 雷一明, 张洁, 王京阳 |
|
High-Throughput Preparation and Corrosion Resistance of Yb-Gd Modified Si Bond Coat |
| WANG Yehan, LV Xirui, SHI Jinyu, LEI Yiming, ZHANG Jie, WANG Jingyang |
| 图5 特征点在组合材料芯片上的位置、1300 ℃空气氧化后微区XRD谱以及表面和截面SEM像 |
| Fig.5 Schematic of L4, F6, and A2 sample patch positions on the material chip (a); micro-XRD patterns of material chips after air oxidation at 1300 oC (b); and surface (c, e, g) and cross-sectional (d, f, h) SEM images of L4 (c, d), F6 (e, f), and A2 (g, h) sample patches after oxidation at 1300 oC (Insets in Figs.5c, e, and g are the corresponding enlarged images) |
|