Yb-Gd改性硅黏结层的高通量制备与耐腐蚀性能 |
| 王晔晗, 吕熙睿, 石金瑜, 雷一明, 张洁, 王京阳 |
|
High-Throughput Preparation and Corrosion Resistance of Yb-Gd Modified Si Bond Coat |
| WANG Yehan, LV Xirui, SHI Jinyu, LEI Yiming, ZHANG Jie, WANG Jingyang |
| 图3 不同Gd / Yb (原子比,下同)样品及Gd / Si样品(RE / Si = 0.6)的微区XRD谱 |