耐事故燃料包壳用FeCrAl合金的腐蚀与辐照性能研究进展
杜东海, 林腾鸿, 王辉

Research Progress on Corrosion and Irradiation Performance of Accident-Tolerant Fuel Cladding FeCrAl Alloy
DU Donghai, LIN Tenghong, WANG Hui
图11 辐照后ODS-FeCrAl合金Al2O3氧化膜中Y-Zr在晶界的分布[178](ODS表示氧化物弥散强化)
Fig.11 Bright field (BF) TEM (a) and high-angle annular dark-field (HAADF) (b) images of distribution of Y-Zr at alumina GBs in ODS-FeCrAl Al2O3 oxide film after irradiation[178] (ODS—oxide dispersion-strengthened)