耐事故燃料包壳用FeCrAl合金的腐蚀与辐照性能研究进展
杜东海, 林腾鸿, 王辉

Research Progress on Corrosion and Irradiation Performance of Accident-Tolerant Fuel Cladding FeCrAl Alloy
DU Donghai, LIN Tenghong, WANG Hui
图8 400 keV Fe+辐照下辐照剂量和辐照温度对Laves相溶解行为的影响[146]
Fig.8 Effect of irradiation dose and temperature on the dissolution of Laves phase under 400 keV Fe+ irradiation[146]