耐事故燃料包壳用FeCrAl合金的腐蚀与辐照性能研究进展 |
| 杜东海, 林腾鸿, 王辉 |
|
Research Progress on Corrosion and Irradiation Performance of Accident-Tolerant Fuel Cladding FeCrAl Alloy |
| DU Donghai, LIN Tenghong, WANG Hui |
| 图7 辐照后不同类型FeCrAl合金中αʹ析出相的数量密度及其与Cr、Al含量的关系[ |
| Fig.7 Number densities of αʹ precipitate densities for each Gen II type FeCrAl alloy (a) and as a function of Cr (b) and Al (c) contents in FeCrAl alloys after radiation at 7 dpa[ |
|