耐事故燃料包壳用FeCrAl合金的腐蚀与辐照性能研究进展 |
| 杜东海, 林腾鸿, 王辉 |
|
Research Progress on Corrosion and Irradiation Performance of Accident-Tolerant Fuel Cladding FeCrAl Alloy |
| DU Donghai, LIN Tenghong, WANG Hui |
| 图6 FeCrAl合金的位错环尺寸以及<100>与1/2<111>位错环中值尺寸之比随辐照剂量的变化[ |
| Fig.6 Loop image sizes for each Burgers vector (a) and ratio of <100> to 1/2<111> median loop size (b) as a function of irradiation dose[ |
|