Arc melting[24-26] | Coarse as-cast structure;microsegregation;shrinkage cavities;limited Nbss continuity control | Mature process;flexible alloy design;convenient for composition exploration | Inhomogeneous solidification;casting defects;limited ingot size | Alloy preparation; composition optimization; phase analysis |
Powder metallurgy[5,15,21] | Refined grains;high densification;uniform phase distribution | Grain refinement; defect reduction; improved microstructure homogeneity | High powder cost; bulk size limit; complex processing | Dense bulk alloy fabrication; fine-grained design |
Directional solidification[5,19,20] | Refined silicides; ordered phase alignment; directional Nbss/silicides distribution | Excellent high-temperature strength, creep resistance; directional load-bearing | Narrow processing window; strict equipment control; poor room-temperature toughness | High-temperature alloy development; creep-resistant design |
Additive manufacturing[5,18,23] | Ultrafine structure;reduced dendrite spacing; enhanced Nbss continuity | Near-net shaping of complex parts; strong grain refinement; rapid composition iteration | High residual stress; pronounced anisotropy; unstable process parameters | Complex component fabrication; rapid alloy development |