合金化调控Nb-Si基超高温合金强韧化与抗氧化性能的研究进展
李云龙, 张子润, 于君, 赵占勇, 林鑫, 白培康

Research Progress on Alloying Regulation of Strengthening, Toughening, and Oxidation Resistance in Nb-Si-Based Ultrahigh-Temperature Alloys
LI Yunlong, ZHANG Zirun, YU Jun, ZHAO Zhanyong, LIN Xin, BAI Peikang
图11 Mo与Zr对Nb-Si基超高温合金力学性能及高温抗氧化性能的协同影响[71]
Fig.11 Synergistic effects of Mo and Zr on mechanical properties and high-temperature oxidation resistance of Nb-Si-based ultrahigh-temperature alloys[71]
(a1-a5) KQ (a1) and fracture surface morphologies of 0Mo-0Zr (a2), 5Mo-0Zr (a3), 0Mo-4Zr (a4), and 5Mo-4Zr (a5) alloys
(b1-b5) high-temperature compression stress-strain curves (b1) and deformation microstructures of 0Mo-0Zr (b2), 5Mo-0Zr (b3), 0Mo-4Zr (b4), and 5Mo-4Zr (b5) alloys
(c1-c5) oxidation mass gain (c1) and microstructures of oxide layers of 0Mo-0Zr (c2), 5Mo-0Zr (c3), 0Mo-4Zr (c4), and 5Mo-4Zr (c5) alloys