合金化调控Nb-Si基超高温合金强韧化与抗氧化性能的研究进展 |
| 李云龙, 张子润, 于君, 赵占勇, 林鑫, 白培康 |
|
Research Progress on Alloying Regulation of Strengthening, Toughening, and Oxidation Resistance in Nb-Si-Based Ultrahigh-Temperature Alloys |
| LI Yunlong, ZHANG Zirun, YU Jun, ZHAO Zhanyong, LIN Xin, BAI Peikang |
| 图9 添加Zr对Nb-Si基超高温合金高温抗氧化性能的影响[ |
| Fig.9 Effects of Zr addition on high-temperature oxidation resistance of Nb-Si-based ultrahigh-temperature alloys[ (a1, a2) weight gain versus time (a1) and the square root of time (a2)(b) macroscopic morphologies before and after oxidation at 1300 oC for 100 h(c1-c5) cross-sectional SEM images of the oxide layer in 0Zr (c1), 1Zr (c2), 3Zr (c3), 5Zr (c4), and 7Zr (c5) alloys(d) BSE image and corresponding EDS elemental mappings of the oxide layer |
|