合金化调控Nb-Si基超高温合金强韧化与抗氧化性能的研究进展
李云龙, 张子润, 于君, 赵占勇, 林鑫, 白培康

Research Progress on Alloying Regulation of Strengthening, Toughening, and Oxidation Resistance in Nb-Si-Based Ultrahigh-Temperature Alloys
LI Yunlong, ZHANG Zirun, YU Jun, ZHAO Zhanyong, LIN Xin, BAI Peikang
图7 不同Zr含量电弧熔炼Nb-16Si-22Ti-2Al-2Cr合金的力学性能[59]
Fig.7 Mechanical properties of Nb-16Si-22Ti-2Al-2Cr alloy with different Zr contents obtained by arc melting[59]
(a) loading-displacement curves(b) room-temperature fracture toughness (KQ)(c) volume fractions of constituent phases(d) true stress-strain curves(e) high-temperature compression strengths and variable quantities