原位自生硼化物增强高强-高导铜基复合材料设计与制备
梁淑华, 姜伊辉, 石浩, 曹飞

Design and Fabrication of High-Strength, High-Conductivity Copper Matrix Composites Reinforced with In Situ-Formed Borides
LIANG Shuhua, JIANG Yihui, SHI Hao, CAO Fei
图4 粉末冶金成形多级构型铜基复合材料的组织和性能[5,13,18,20]
Fig.4 Microstructures and properties of hierarchical architected copper matrix composites fabricated by powder metallurgy
(a) low magnification TEM image showing the micro-clusters of TiB2 particles[18]
(b) high magnification TEM image showing the nano-precipitates[18]
(c) HRTEM image of coherent nano-precipitates[18]
(d) SAED pattern of coherent nano-precipitates of square region in Fig.4c[18]
(e) interaction between dislocations and TiB2 clusters obtained by dislocation extraction algorithm method (ε—strain. Insets show the locally enlarged images of square regions)[18]
(f) plot of tensile strength versus electrical conductivity for different copper-based materials[5,13,18,20]