原位自生硼化物增强高强-高导铜基复合材料设计与制备
梁淑华, 姜伊辉, 石浩, 曹飞

Design and Fabrication of High-Strength, High-Conductivity Copper Matrix Composites Reinforced with In Situ-Formed Borides
LIANG Shuhua, JIANG Yihui, SHI Hao, CAO Fei
图3 原位自生铜基复合材料粉末制备原理及其宏、微观特征[15,18]
Fig.3 Preparation principle of in situ copper matrix composite powders and their macro- and micro-structure characteristics
(a) illustration of in situ reaction and gas atomization process[15]
(b) macrostructure characteristics of TiB2/Cu composite powders
(c) powder size distribution and morphology (inset)[18]
(d) surface topography and detailed view (inset)[18]
(e) 3D rendering nano-CT image showing the TiB2 particles micro-clusters[18]
(f) XRD pattern of the TiB2/Cu composite powders[18]