高强钢焊缝金属强韧性研究进展
曹睿, 刘梓申

Research Progress on the Strength and Toughness of High-Strength Steel Weld Metal
CAO Rui, LIU Zishen
表1 高强钢焊缝金属显微组织含量与C当量的关系[8]
Table 1 Relationship between volume fraction of microstructure and carbon equivalent (CE) of high-strength steel weld metals[8]
CEfAF / %fGB / %fBU / %fBL / %fLM / %
0.240-0.26520-45≈ 1020-30530-50
0.265-0.27510-201015-25550-65
0.272-0.2855-151010-20560-75
0.285-0.2955-12510-15570-85
0.293-0.30010510580-95
0.300005595-100