高强钢焊缝金属强韧性研究进展 |
| 曹睿, 刘梓申 |
|
Research Progress on the Strength and Toughness of High-Strength Steel Weld Metal |
| CAO Rui, LIU Zishen |
| 图6 预回火对高强钢焊缝金属显微组织和冲击韧性的影响[ |
| Fig.6 Effects of pre-tempering on microstructure and impact toughness of high-strength steel weld metal[ (a1-a3) heat treatment process diagrams of tempered (types II and III) (a1, a2) and pre-tempered + tempered (type IV) (a3) (b) impact energies of types I-IV weld metals (type I—as-welded) (c1-c4) microstructures of types I (c1), II (c2), III (c3), and IV (c4) weld metals |
|