| 张林杰, 张栩菁, 宁杰 |
|
Research Progress on the High-Temperature Creep Properties of Molybdenum Alloy Welded Joints |
| ZHANG Linjie, ZHANG Xujing, NING Jie |
| 图3 典型的钼合金焊接断口以及钼合金母材蠕变裂纹[ |
| Fig.3 High (a, c) and low (b, d) magnified morphologies showing typical tensile fracture of molybdenum alloy welding[ |
|