电弧增材制造高强度Al-Mg-Sc系合金研究进展:冶金缺陷、微观组织和力学性能
马成勇, 侯旭儒, 赵琳, 阚成玲, 曹洋, 彭云, 田志凌

Research Progress on High-Strength Al-Mg-Sc Alloys Fabricated by Wire Arc Additive Manufacturing: Metallurgical Defects, Microstructure, and Performance
MA Chengyong, HOU Xuru, ZHAO Lin, KAN Chengling, CAO Yang, PENG Yun, TIAN Zhiling
图15 基于增强学习的WAAM缺陷监测流程[77]
Fig.15 Defect monitoring process based on reinforcement learning in WAAM[77]
(a) data collection
(b) feature extraction
(c, d) support vector machines (SVM) classification results