冷丝辅助旋转/摇动电弧窄间隙MAG焊缝成形特性及接头组织性能演变机制
李红, 姜玉清, 曹玉鹏, 王加友, 刘澍彬

Weld Formation Characteristics and the Evolution Mechanisms of Joint Microstructure and Mechanical Properties for Rotating/Swing Arc Narrow Gap MAG Welding Assisted by Cold Wire
LI Hong, JIANG Yuqing, CAO Yupeng, WANG Jiayou, LIU Shubin
图10 窄间隙多层焊第三层焊缝右侧FL区组织的EBSD分析结果
Fig.10 EBSD analysis results of the microstructure in the region neighboring FL on the right side of the 3rd-layer narrow gap weld by RA (a,a1, a2), RA + CW (b, b1, b2), SA (c, c1, c2), and SA + CW (d, d1, d2); statistics of average grain size (e), misorientation angle distributions of WMFL3 (f) and CGHAZ (g), and texture strength (h) (CGHAZ—coarse-grain heat-affected zone, FGHAZ—fine-grain heat-affected zone, HAGB—high angle grain boundary, LAGB—low angle grain boundary) (a-d) inverse pole figures (IPFs) for WMFL3 and CGHAZ (a1-d1) pole figures (PFs) for WMFL3 (a2-d2) PFs for CGHAZ