冷丝辅助旋转/摇动电弧窄间隙MAG焊缝成形特性及接头组织性能演变机制 |
| 李红, 姜玉清, 曹玉鹏, 王加友, 刘澍彬 |
|
Weld Formation Characteristics and the Evolution Mechanisms of Joint Microstructure and Mechanical Properties for Rotating/Swing Arc Narrow Gap MAG Welding Assisted by Cold Wire |
| LI Hong, JIANG Yuqing, CAO Yupeng, WANG Jiayou, LIU Shubin |
| 图8 冷丝辅助旋转/摇动电弧窄间隙MAG多层焊接头形貌(L1~L6分别表示第1至第6层焊缝) |
| Fig.8 Morphologies of rotating/swing arc narrow gap MAG multi-layer welding joint assisted by CW (WMNRH3—non-reheated region of the 3rd-layer weld metal, RHAZ43—reheated affected zone (in the 3rd-layer weld) induced by the 4th-layer weld, RHAZ32—reheated affected zone (in the 2nd-layer weld) induced by the 3rd-layer weld; L1-L6 denote weld layers, and areas 1-3 indicate EBSD observing regions) (a) rotating arc for single wire (RA) (b) RA + CW (c) swing arc for single wire (SA) (d) SA + CW |
|