低碳钢预制涡流搅拌摩擦焊工艺研究
王启勇, 李晓博, 刘小超, 王心成, 张泰瑞, 倪中华, 陈彪

Process of Prefabricated Vortex Flow-Based Friction Stir Welding for Low Carbon Steel
WANG Qiyong, LI Xiaobo, LIU Xiaochao, WANG Xincheng, ZHANG Tairui, NI Zhonghua, CHEN Biao
表1 WC-Co和W-Re系合金的性能[25~29]
Table 1 Properties for WC-Co and W-Re alloys[25-29]
AlloyCoefficient of frictionThermal conductivity / (W·m-1·K-1)Flow stress
WC-(13, 17)Co0.4[25]124-130[26]620-750 MPa at 900 oC[27]
W-25Re0.52[28]55-65[29]500-800 MPa at 1000 oC[29]