低碳钢预制涡流搅拌摩擦焊工艺研究 |
| 王启勇, 李晓博, 刘小超, 王心成, 张泰瑞, 倪中华, 陈彪 |
|
Process of Prefabricated Vortex Flow-Based Friction Stir Welding for Low Carbon Steel |
| WANG Qiyong, LI Xiaobo, LIU Xiaochao, WANG Xincheng, ZHANG Tairui, NI Zhonghua, CHEN Biao |
| 图12 WC-Co和W-Re套筒在最优参数条件下所获接头横截面的显微硬度分布云图及曲线 |
| Fig.12 Microhardness contour maps (a, b) and distribu-tion profiles along line 1 and line 2 (c) of the cross-section of joints prepared by different holders under corresponding optimal parameters (a) WC-Co holder (b) W-Re holder |
|