34CrNi1Mo/Q355B异种钢对接接头残余应力及焊后热处理对残余应力的影响
瞿铁, 谢杨, 王重阳, 李利霞, 徐侠剑, 毛峙溆, 骆文泽, 黄智泉, 邓德安

Residual Stress in a 34CrNi1Mo/Q355B Dissimilar Steel Butt Joint and the Effects of Post-Weld Heat Treatment on Residual Stress
QU Tie, XIE Yang, WANG Chongyang, LI Lixia, XU Xiajian, MAO Zhixu, LUO Wenze, HUANG Zhiquan, DENG Dean
表1 34CrNi1Mo钢和Q355B钢母材及ER50-6和H10Mn2焊丝的化学成分
Table 1 Chemical compositions of 34CrNi1Mo and Q355B steel base materials and ER50-6 and H10Mn2 welding wires (mass fraction / %)
MaterialCSiMnCrNiMoSPFe
34CrNi1Mo0.300.200.501.301.300.15≤ 0.035≤ 0.035Bal.
Q355B0.200.500.900.300.30-≤ 0.035≤ 0.035Bal.
ER50-60.151.151.850.150.150.15≤ 0.025≤ 0.025Bal.
H10Mn20.120.071.900.200.30-≤ 0.035≤ 0.035Bal.