34CrNi1Mo/Q355B异种钢对接接头残余应力及焊后热处理对残余应力的影响
瞿铁, 谢杨, 王重阳, 李利霞, 徐侠剑, 毛峙溆, 骆文泽, 黄智泉, 邓德安

Residual Stress in a 34CrNi1Mo/Q355B Dissimilar Steel Butt Joint and the Effects of Post-Weld Heat Treatment on Residual Stress
QU Tie, XIE Yang, WANG Chongyang, LI Lixia, XU Xiajian, MAO Zhixu, LUO Wenze, HUANG Zhiquan, DENG Dean
图15 Case B~D中34CrNi1Mo与Q355B钢对接接头的下表面及中央截面焊缝附近的纵向残余应力分布云图
Fig.15 Contours of longitudinal residual stress distribution on the lower surface (a1-c1) and middle cross-section near the weld (a2-c2) of 34CrNi1Mo and Q355B butt joint in case B (a1, a2), case C (b1, b2), and case D (c1, c2)