34CrNi1Mo/Q355B异种钢对接接头残余应力及焊后热处理对残余应力的影响 |
| 瞿铁, 谢杨, 王重阳, 李利霞, 徐侠剑, 毛峙溆, 骆文泽, 黄智泉, 邓德安 |
|
Residual Stress in a 34CrNi1Mo/Q355B Dissimilar Steel Butt Joint and the Effects of Post-Weld Heat Treatment on Residual Stress |
| QU Tie, XIE Yang, WANG Chongyang, LI Lixia, XU Xiajian, MAO Zhixu, LUO Wenze, HUANG Zhiquan, DENG Dean |
| 图13 Case A和Case B中34CrNi1Mo与Q355B钢对接接头的上表面及中央截面焊缝附近的横向残余应力分布云图 |
| Fig.13 Contours of transverse residual stress distribution on the top surface (a1, b1) and middle cross-sections near the weld (a2, b2) of 34CrNi1Mo and Q355B butt joint in case A (a1, a2) and case B (b1, b2) |
|