34CrNi1Mo/Q355B异种钢对接接头残余应力及焊后热处理对残余应力的影响 |
| 瞿铁, 谢杨, 王重阳, 李利霞, 徐侠剑, 毛峙溆, 骆文泽, 黄智泉, 邓德安 |
|
Residual Stress in a 34CrNi1Mo/Q355B Dissimilar Steel Butt Joint and the Effects of Post-Weld Heat Treatment on Residual Stress |
| QU Tie, XIE Yang, WANG Chongyang, LI Lixia, XU Xiajian, MAO Zhixu, LUO Wenze, HUANG Zhiquan, DENG Dean |
| 图9 34CrNi1Mo钢微观组织的OM像 |
| Fig.9 OM images of 34CrNi1Mo steel (a) coarse grain HAZ (b) fine grain HAZ (c) inter-critical HAZ (d) base metal |
|