34CrNi1Mo/Q355B异种钢对接接头残余应力及焊后热处理对残余应力的影响
瞿铁, 谢杨, 王重阳, 李利霞, 徐侠剑, 毛峙溆, 骆文泽, 黄智泉, 邓德安

Residual Stress in a 34CrNi1Mo/Q355B Dissimilar Steel Butt Joint and the Effects of Post-Weld Heat Treatment on Residual Stress
QU Tie, XIE Yang, WANG Chongyang, LI Lixia, XU Xiajian, MAO Zhixu, LUO Wenze, HUANG Zhiquan, DENG Dean
图3 34CrNi1Mo钢的热物性参数
Fig.3 Thermal physical property parameters of 34CrNi1Mo steel