316H钢及其焊缝金属辐照He泡演化与力学行为的相场-晶体塑性耦合模拟
王栋, 徐连勇, 赵雷, 韩永典, 宋恺

Phase Field and Crystal Plasticity Simulation of Irradiation-Induced He Bubbles Evolution and Mechanical Behavior in 316H Steel and Weld Metal
WANG Dong, XU Lianyong, ZHAO Lei, HAN Yongdian, SONG Kai
表2 He泡相场模拟中所用的热力学参数[12,32~34]
Table 2 Thermodynamic parameters used in phase field simulation[12,32-34]
ParameterValueUnit
Va[32]7.06cm3·mol-1
Evf[12]3.2 × 10-19J
Egf[12]6.4 × 10-19J
Ω[32]1.17 × 10-29m3
bv[33]0.039nm3·atom-1
a[33]0.0034J·m3·mol-2
γs[34]1.82J·m-2