316H钢及其焊缝金属辐照He泡演化与力学行为的相场-晶体塑性耦合模拟
王栋, 徐连勇, 赵雷, 韩永典, 宋恺

Phase Field and Crystal Plasticity Simulation of Irradiation-Induced He Bubbles Evolution and Mechanical Behavior in 316H Steel and Weld Metal
WANG Dong, XU Lianyong, ZHAO Lei, HAN Yongdian, SONG Kai
表1 316H钢母材及焊丝的化学成分 (mass fraction / %)
Table 1 Chemical compositions of the 316H base metal and welding wuire
MaterialCrNiMnMoSiCoCNFe
316H17.2412.171.812.560.370.0190.0470.064Bal.
Welding wire18.7012.801.672.320.490.0080.0520.057Bal.