316H钢及其焊缝金属辐照He泡演化与力学行为的相场-晶体塑性耦合模拟 |
| 王栋, 徐连勇, 赵雷, 韩永典, 宋恺 |
|
Phase Field and Crystal Plasticity Simulation of Irradiation-Induced He Bubbles Evolution and Mechanical Behavior in 316H Steel and Weld Metal |
| WANG Dong, XU Lianyong, ZHAO Lei, HAN Yongdian, SONG Kai |
| 图13 He泡占比和尺寸对应力-应变曲线的影响 |
| Fig.13 Effects of He bubble porosity (a, c) and size (b, d) in 316H steel (a, b) and 316H WM (c, d) on stress-strain curves unde 550 oC (The circular areas in Figs.13a and c imply the applied strain begins to dominate the mechanical response) |
|