316H钢及其焊缝金属辐照He泡演化与力学行为的相场-晶体塑性耦合模拟
王栋, 徐连勇, 赵雷, 韩永典, 宋恺

Phase Field and Crystal Plasticity Simulation of Irradiation-Induced He Bubbles Evolution and Mechanical Behavior in 316H Steel and Weld Metal
WANG Dong, XU Lianyong, ZHAO Lei, HAN Yongdian, SONG Kai
图10 316H钢母材的焊缝金属He泡直径及其分布的相场模拟与实验定量统计对比
Fig.10 Quantitative statistical comparisons of diameter evolution (a, c) and diameter distribution (He concentration is 0.04) (b, d) of He bubbles in 316H steel (a, b) and 316H WM (c, d)