316H钢及其焊缝金属辐照He泡演化与力学行为的相场-晶体塑性耦合模拟 |
| 王栋, 徐连勇, 赵雷, 韩永典, 宋恺 |
|
Phase Field and Crystal Plasticity Simulation of Irradiation-Induced He Bubbles Evolution and Mechanical Behavior in 316H Steel and Weld Metal |
| WANG Dong, XU Lianyong, ZHAO Lei, HAN Yongdian, SONG Kai |
| 图6 辐照条件下多个He泡的演变 |
| Fig.6 Evolutions of multiple He bubbles under irradiation (a-d) He concentration fields under He concentrations of 0.007 (a), 0.01 (b), 0.015 (c), and 0.04 (d) (e-h) vacancy concentration fields under He concentrations of 0.007 (e), 0.01 (f), 0.015 (g), and 0.04 (h) (The circular area B in Fig.6g implies the Ostwald ripening and the elliptical area A in Fig.6h implies the coalescence) |
|