316H钢及其焊缝金属辐照He泡演化与力学行为的相场-晶体塑性耦合模拟
王栋, 徐连勇, 赵雷, 韩永典, 宋恺

Phase Field and Crystal Plasticity Simulation of Irradiation-Induced He Bubbles Evolution and Mechanical Behavior in 316H Steel and Weld Metal
WANG Dong, XU Lianyong, ZHAO Lei, HAN Yongdian, SONG Kai
图5 过饱和基体中单个He泡的演变
Fig.5 Evolution of a single bubble in the supersaturated matrix (The color bar implies the values of He concentration (cg) and vancay concentration (cv), the same in Fig.6; Δx*—dimexsionless length scale)
(a-c) He concentration fields under t* = 0 (a), t* = 10 (b), and t* = 80 (c) (t*—dimensionless time) (d-f) vacancy concentration fields under t* = 0 (d), t* = 10 (e), and t* = 80 (f) (g-i) profiles of He and vacancy concentrations across the He bubble under t* = 0 (g), t* = 10 (h), and t* = 80 (i)