铝合金搅拌摩擦焊热-力-流耦合仿真及材料迁移轨迹解析 |
| 韩鸿华, 史清宇, 杨诚乐, 孔德帅, 陈高强 |
|
Coupled Thermal-Mechanical-Fluid Simulation and Material Migration Trajectory Analysis for Friction Stir Welding of Aluminum Alloy |
| HAN Honghua, SHI Qingyu, YANG Chengle, KONG Deshuai, CHEN Gaoqiang |
| 图12 起始于Y = 1.2 mm、Z = 3 mm的直通流动路径及其Z向速度分布 |
| Fig.12 Straight-through flow paths initiated at Y = 1.2 mm, Z = 3 mm and its Z-direction velocity distribution (a) 3D view (b) X-Y view (c) X-Z view |
|