铝合金搅拌摩擦焊热-力-流耦合仿真及材料迁移轨迹解析 |
| 韩鸿华, 史清宇, 杨诚乐, 孔德帅, 陈高强 |
|
Coupled Thermal-Mechanical-Fluid Simulation and Material Migration Trajectory Analysis for Friction Stir Welding of Aluminum Alloy |
| HAN Honghua, SHI Qingyu, YANG Chengle, KONG Deshuai, CHEN Gaoqiang |
| 图8 Z = 7 mm和Z = 3 mm平面材料流动轨迹的分布 |
| Fig.8 Distributions of the material flow trajectory at Z = 7 mm plane (a-c) and Z = 3 mm plane (d-f) (a, d) overall views (b, e) AS (c, f) RS |
|