铝合金搅拌摩擦焊热--流耦合仿真及材料迁移轨迹解析
韩鸿华, 史清宇, 杨诚乐, 孔德帅, 陈高强

Coupled Thermal-Mechanical-Fluid Simulation and Material Migration Trajectory Analysis for Friction Stir Welding of Aluminum Alloy
HAN Honghua, SHI Qingyu, YANG Chengle, KONG Deshuai, CHEN Gaoqiang
图3 FSW过程中工件表面的温度分布预测结果,X = 0 mm截面上的温度分布,及热电偶安装处温度仿真结果与实测结果
Fig.3 Simulated temperature distributions of full workpiece surface (a) and X = 0 mm section (b), and simulated and measured temperatures of AS (c) and RS (d) during FSW (Tmax—maximum simulated temperature of the workpiece; TAS_max, TRS_max—maximum temperatures on the AS and RS of the X = 0 section, respectively; Tmax.Sim., Tmax.Exp.—maximum simulated and experimentally measured temperatures at the thermocouple location, respectively)