超声振动对镁/铝异质合金搅拌摩擦搭接焊接头界面组织演变的影响
阴嘉琳, 石磊, 武传松

Effect of Ultrasonic Vibration on Microstructure Evolution at the Mg/Al Dissimilar Alloy Friction Stir Welded Lap Joint Interface
YIN Jialin, SHI Lei, WU Chuansong
表1 母材化学成分 (mass fraction / %)
Table 1 Chemical compositions of base materials
AlloySiFeCuMnZnCrAlMg
AZ31B-H24 Mg0.00640.00650.00010.0030.680-2.68Bal.
6061-T6 Al0.64900.60000.21500.1320.2450.095Bal.1.02