超声振动对镁/铝异质合金搅拌摩擦搭接焊接头界面组织演变的影响
阴嘉琳, 石磊, 武传松

Effect of Ultrasonic Vibration on Microstructure Evolution at the Mg/Al Dissimilar Alloy Friction Stir Welded Lap Joint Interface
YIN Jialin, SHI Lei, WU Chuansong
图15 UVeFSLW接头镁合金侧水平截面过匙孔中心焊接路径上特征区域的IPFs
Fig.15 Horizontal cross-sectional IPFs of characteristic regions in Fig.5b along the welding path through the keyhole center on the Mg alloy side of the UVeFSLW joint
(a) C2 (b) C1 (c) C (d) G (e) G1 (f) G2