超声振动对镁/铝异质合金搅拌摩擦搭接焊接头界面组织演变的影响 |
| 阴嘉琳, 石磊, 武传松 |
|
Effect of Ultrasonic Vibration on Microstructure Evolution at the Mg/Al Dissimilar Alloy Friction Stir Welded Lap Joint Interface |
| YIN Jialin, SHI Lei, WU Chuansong |
| 图9 围绕匙孔中心不同角度样品垂直截面的OM像 |