超声振动对镁/铝异质合金搅拌摩擦搭接焊接头界面组织演变的影响
阴嘉琳, 石磊, 武传松

Effect of Ultrasonic Vibration on Microstructure Evolution at the Mg/Al Dissimilar Alloy Friction Stir Welded Lap Joint Interface
YIN Jialin, SHI Lei, WU Chuansong
图7 不同参数和工艺下搭接接头的有效板厚(dEST)
Fig.7 dEST of lap joints under various parameters and processes
(a) welding speed 90 min/mm (b) rotation speed 800 r/min