图3 TiAl/Ti33.3Zr16.7Cu39Ni11/GH3030接头在960 ℃钎焊10 min后显微组织的SEM像[40]
Fig.3 SEM images of TiAl/Ti33.3Zr16.7Cu39Ni11/GH3030 joint brazed at 960 oC for 10 min[40]
(a) TiAl/Ti33.3Zr16.7Cu39Ni11 interface (b) tolal view of joint (c) Ti33.3Zr16.7Cu39Ni11/GH3030 interface