异种金属钎焊连接研究进展
曹健, 高建伟, 赵文笛, 薛鹏鹏, 杨博, 李淳, 亓钧雷, 司晓庆

Research Progress on Brazing of Dissimilar Metals
CAO Jian, GAO Jianwei, ZHAO Wendi, XUE Pengpeng, YANG Bo, LI Chun, QI Junlei, SI Xiaoqing
图2 BNi-2钎料在TC4母材上润湿铺展过程中的代表性瞬时照片[35]
Fig.2 Representative instantaneous images of the wetting and spreading processes of BNi-2 (Cr-7Si-3B) filler metal on TC4 substrate[35] (T—temperature, t—time)
(a) 1020 oC (b) 1080 oC (c) 1150 oC