固相摩擦增材制造技术研究进展及其应用现状
刘海滨, 张迎星, 谢瑞山, 陈树君

Recent Research Progress in Solid-State Friction-Based Additive Manufacturing Technology and Its Current Applications
LIU Haibin, ZHANG Yingxing, XIE Ruishan, CHEN Shujun
图14 利用FRAM技术制备的多种典型构件:单壁构件、铝合金圆柱体[54]、U型样件、十字交叉样件、C型样件、大型圆环构件、铝/钢异质结构[57]及高筋板壁板样品[93]
Fig.14 Several typical components fabricated using FRAM technology
(a) single-walled member (b) aluminum alloy cylinder[54]
(c) U-shaped sample (d) criss-cross sample
(e) C-shaped sample (f) large circular member
(g) aluminum/steel heterogeneous structure[57] (h) sample of high-bar plate siding[93]