固相摩擦增材制造技术研究进展及其应用现状 |
| 刘海滨, 张迎星, 谢瑞山, 陈树君 |
|
Recent Research Progress in Solid-State Friction-Based Additive Manufacturing Technology and Its Current Applications |
| LIU Haibin, ZHANG Yingxing, XIE Ruishan, CHEN Shujun |
| 图9 FRAM、预热FRAM (P-FRAM)和预热-水冷辅助FRAM (PC-FRAM)三种工艺沉积试样在yz平面上的硬度测试结果[ |
| Fig.9 Hardness results on yz-plane of three samples deposited via different processes[ (a) FRAM (b) preheating FRAM (P-FRAM) (c) preheating and water-cooling-assisted FRAM (PC-FRAM) |
|