高强钢焊缝金属组织设计与强韧化机理研究进展
陆善平, 孙健

Research Progress on Microstructural Design and Strengthening-Toughening Mechanisms of Weld Metal in High-Strength Steels
LU Shanping, SUN Jian
图2 夹杂物种类计算与夹杂物实验表征[24]
Fig.2 Calculation of inclusion types and experimental characterization of the inclusion[24]
(a) thermodynamic calculation results (b1, b2) TEM image (b1) and line scan results in Fig.2b1 (b2) (MDZ—Mn-depleted zone)