高强钢焊缝金属组织设计与强韧化机理研究进展
陆善平, 孙健

Research Progress on Microstructural Design and Strengthening-Toughening Mechanisms of Weld Metal in High-Strength Steels
LU Shanping, SUN Jian
图1 Ti含量对焊缝金属中夹杂物的影响[19]
Fig.1 Effect of Ti contents on the inclusions in weld metals[19]
(a) 0.0028%Ti (b) 0.0255%Ti